S-Plastics Ultem JD7902 resin
| MECHANICAL | Value | Unit | Standard |
| Tensile Stress, yield | 127 | MPa | S-Plastics - Japan Method |
| Tensile Strain, break | 5 - 5 | % | S-Plastics - Japan Method |
| Flexural Stress | 186 | MPa | ASTM D 790 |
| Flexural Modulus | 5880 | MPa | ASTM D 790 |
| IMPACT | Value | Unit | Standard |
| Izod Impact, notched, 23°C | 49 | J/m | ASTM D 256 |
| THERMAL | Value | Unit | Standard |
| HDT, 0.45 MPa, 3.2 mm, unannealed | 210 | °C | ASTM D 648 |
| CTE, -30°C to 30°C | 3.5E-05 - 3.5E-05 | 1/°C | TMA |
| PHYSICAL | Value | Unit | Standard |
| Specific Gravity | 1.38 | - | ASTM D 792 |
| Water Absorption, 24 hours | 0.26 | % | ASTM D 570 |
| Mold Shrinkage, flow, 3.2 mm | 0.3 - 0.5 | % | S-Plastics Method |
| ELECTRICAL | Value | Unit | Standard |
| Surface Resistivity | 1.E+06 - 1.E+08 | Ohm | ASTM D 257 |
| Source GMD, last updated:02/01/2000 |
|
For more information please download the datasheet |
|
| S-Plastics Ultem JD7902.pdf | |
|