TYPICAL PROPERTIES (1) | |||
MECHANICAL | Value | Unit | Standard |
Tensile Stress, yld, Type I, 5 mm/min | 60 | MPa | ASTM D 638 |
Tensile Stress, brk, Type I, 5 mm/min | 59 | MPa | ASTM D 638 |
Tensile Strain, yld, Type I, 5 mm/min | 3.7 | % | ASTM D 638 |
Tensile Modulus, 5 mm/min | 4700 | MPa | ASTM D 638 |
Tensile Stress, yield, 5 mm/min | 59 | MPa | ISO 527 |
Tensile Stress, break, 5 mm/min | 47 | MPa | ISO 527 |
Tensile Strain, yield, 5 mm/min | 3.6 | % | ISO 527 |
Tensile Strain, break, 5 mm/min | 64 | % | ISO 527 |
Tensile Modulus, 1 mm/min | 4470 | MPa | ISO 527 |
Flexural Stress, yield, 2 mm/min | 100 | MPa | ISO 178 |
Flexural Modulus, 2 mm/min | 4200 | MPa | ISO 178 |
IMPACT | Value | Unit | Standard |
Instrumented Impact Total Energy, 23°C | 60 | J | ASTM D 3763 |
Izod Impact, notched 80*10*3 +23°C | 14 | kJ/m² | ISO 180/1A |
Izod Impact, notched 80*10*3 -30°C | 7 | kJ/m² | ISO 180/1A |
Charpy 23°C, V-notch Edgew 80*10*3 sp=62mm | 37 | kJ/m² | ISO 179/1eA |
Charpy -30°C, V-notch Edgew 80*10*3 sp=62mm | 10 | kJ/m² | ISO 179/1eA |
THERMAL | Value | Unit | Standard |
HDT, 1.82 MPa, 3.2mm, unannealed | 124 | °C | ASTM D 648 |
CTE, -40°C to 40°C, flow | 4.E-05 | 1/°C | ASTM E 831 |
CTE, -40°C to 40°C, xflow | 9.E-05 | 1/°C | ASTM E 831 |
CTE, -40°C to 40°C, flow | 4.E-05 | 1/°C | ISO 11359-2 |
CTE, -40°C to 40°C, xflow | 9.E-05 | 1/°C | ISO 11359-2 |
Vicat Softening Temp, Rate B/50 | 137 | °C | ISO 306 |
HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm | 122 | °C | ISO 75/Af |
PHYSICAL | Value | Unit | Standard |
Specific Gravity | 1.27 | - | ASTM D 792 |
Density | 1.27 | g/cm³ | ISO 1183 |
Melt Volume Rate, MVR at 260°C/5.0 kg | 10 | cm³/10 min | ISO 1133 |
Melt Volume Rate, MVR at 265°C/5.0 kg | 12 | cm³/10 min | ISO 1133 |
Source GMD, last updated:2009/08/20 |
Parameter | ||
Injection Molding | Value | Unit |
Drying Temperature | 100 - 110 | °C |
Drying Time | 3 - 4 | hrs |
Maximum Moisture Content | 0.04 | % |
Melt Temperature | 270 - 300 | °C |
Nozzle Temperature | 260 - 290 | °C |
Front - Zone 3 Temperature | 270 - 300 | °C |
Middle - Zone 2 Temperature | 265 - 290 | °C |
Rear - Zone 1 Temperature | 260 - 270 | °C |
Mold Temperature | 60 - 100 | °C |
Back Pressure | 0.3 - 0.7 | MPa |
Screw Speed | 40 - 70 | rpm |
Shot to Cylinder Size | 30 - 80 | % |
Vent Depth | 0.038 - 0.076 | mm |
Source GMD, last updated:2009/08/20 |
For more information please download the datasheet |
|
![]() |
S-Plastics Cycoloy XCM840.pdf |
Get The Latest Quotation
First-level distribution source in South China Reduce procurement costs, improve supply stability, Help you find the most suitable engineering plastic materials
|