S-Plastics Cycoloy EXCY0223 resin
| TYPICAL PROPERTIES (1) | |||
| MECHANICAL | Value | Unit | Standard |
| Tensile Stress, yield, 5 mm/min | 60 | MPa | ISO 527 |
| Tensile Stress, break, 5 mm/min | 46 | MPa | ISO 527 |
| Tensile Strain, yield, 5 mm/min | 4 | % | ISO 527 |
| Tensile Strain, break, 5 mm/min | 8 | % | ISO 527 |
| Tensile Modulus, 1 mm/min | 3550 | MPa | ISO 527 |
| Flexural Stress, yield, 2 mm/min | 98 | MPa | ISO 178 |
| Flexural Modulus, 2 mm/min | 3550 | MPa | ISO 178 |
| IMPACT | Value | Unit | Standard |
| Multiaxial Impact | 80 | J | ISO 6603 |
| THERMAL | Value | Unit | Standard |
| Vicat Softening Temp, Rate B/120 | 132 | °C | ISO 306 |
| HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm | 118 | °C | ISO 75/Af |
| PHYSICAL | Value | Unit | Standard |
| Melt Volume Rate, MVR at 260°C/5.0 kg | 16 | cm³/10 min | ISO 1133 |
| FLAME CHARACTERISTICS | Value | Unit | Standard |
| NBS Smoke Density, Flaming, 4 min (3.2 mm) | 130 | - | ASTM E 662 |
| NBS Smoke Density, Flaming, 20 min (3.2 mm) | 330 | - | ASTM E 662 |
| Source GMD, last updated:09/12/2007 | |||
| Parameter | ||
| Injection Molding | Value | Unit |
| Drying Temperature | 90 - 100 | °C |
| Drying Time | 2 - 4 | hrs |
| Maximum Moisture Content | 0.02 | % |
| Melt Temperature | 250 - 300 | °C |
| Nozzle Temperature | 230 - 290 | °C |
| Front - Zone 3 Temperature | 240 - 300 | °C |
| Middle - Zone 2 Temperature | 230 - 290 | °C |
| Rear - Zone 1 Temperature | 210 - 260 | °C |
| Hopper Temperature | 60 - 80 | °C |
| Mold Temperature | 60 - 90 | °C |
| Source GMD, last updated:09/12/2007 | ||
|
For more information please download the datasheet |
|
| S-Plastics cycoloy EXCY0223.pdf | |
|
Get The Latest Quotation
First-level distribution source in South China Reduce procurement costs, improve supply stability, Help you find the most suitable engineering plastic materials
|
![]()