| Heat Stabilized | Yes |
|---|---|
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Supply Ability | To be negotiated |
| Density | 1.57 |
|---|---|
| Mold Shrinkage, Flow | 0.4 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Density | 1.29 |
|---|---|
| Mold Shrinkage, Flow | 0.3 - 0.6 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Density | 1.43 |
|---|---|
| Mold Shrinkage, Flow | 0.3 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 260°C/2.16 Kgf | 29 |
|---|---|
| Melt Volume Rate, MVR At 260°C/2.16 Kg | 30cm³/10 Min |
| UV PerfoImprovedrmance | Improved |
| Aesthetically And Physically | Improved |
| Packaging Details | 25KG/bag |
| Density | 1.15 |
|---|---|
| Mold Shrinkage, Flow | 0.8 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 8.4 |
|---|---|
| Oxygen Index (LOI) | 50 |
| Glass Fiber | 20% |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Melt Flow Rate, 337°C/6.6 Kgf | 9 |
|---|---|
| Oxygen Index (LOI) | 47 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 11 |
|---|---|
| Electroplatability | Enhanced |
| Mold Release | Internal |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Melt Flow Rate, 337°C/6.6 Kgf | 7.6 |
|---|---|
| Glass Fiber | 30% |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |