S-Plastics Lexan RL6538resin is SINGLE LOT DATA (L37048, 70656 color): High flow, superior release.
MECHANICAL | Value | Unit | Standard |
Tensile Stress, yld, Type I, 50 mm/min | 62 | MPa | ASTM D 638 |
Tensile Stress, brk, Type I, 50 mm/min | 64 | MPa | ASTM D 638 |
Tensile Strain, brk, Type I, 50 mm/min | 85 | % | ASTM D 638 |
Flexural Stress, yld, 1.3 mm/min, 50 mm span | 96 | MPa | ASTM D 790 |
Flexural Modulus, 1.3 mm/min, 50 mm span | 2240 | MPa | ASTM D 790 |
IMPACT | Value | Unit | Standard |
Izod Impact, notched, 23°C | 715 | J/m | ASTM D 256 |
Instrumented Impact Energy @ peak, 23°C | 53 | J | ASTM D 3763 |
THERMAL | Value | Unit | Standard |
HDT, 1.82 MPa, 6.4 mm, unannealed | 122 | °C | ASTM D 648 |
PHYSICAL | Value | Unit | Standard |
Specific Gravity | 1.2 | - | ASTM D 792 |
Melt Flow Rate, 300°C/1.2 kgf | 24.6 | g/10 min | ASTM D 1238 |
Source GMD, last updated:01/04/2000 |
Parameter | ||
Injection Molding | Value | Unit |
Drying Temperature | 105 | °C |
Drying Time | 3 - 4 | hrs |
Drying Time (Cumulative) | 24 | hrs |
Maximum Moisture Content | 0.02 | % |
Melt Temperature | 250 - 270 | °C |
Nozzle Temperature | 245 - 265 | °C |
Front - Zone 3 Temperature | 250 - 270 | °C |
Middle - Zone 2 Temperature | 240 - 260 | °C |
Rear - Zone 1 Temperature | 225 - 250 | °C |
Mold Temperature | 50 - 80 | °C |
Back Pressure | 0.3 - 0.7 | MPa |
Screw Speed | 40 - 70 | rpm |
Shot to Cylinder Size | 40 - 60 | % |
Vent Depth | 0.025 - 0.076 | mm |
Source GMD, last updated:01/04/2000 |