Melt Flow Rate, 220°C/10.0 Kgf: 38
UL Recognized, 94HB Flame Class Rating (3): ???
Basic Infomation
Place of Origin: ——
Brand Name: S-Plastic Geloy
Certification: COA/ICP Test/Rohs/MSDS
Model Number: EXGY0049
Payment & Shipping Terms
Packaging Details: 25KG/bag
Delivery Time: To be negotiated
Payment Terms: L/C, T/T, Western Union, MoneyGram
Supply Ability: To be negotiated
Product Description

S-Plastics Geloy  EXGY004 resin is ASA/PMMA
 


Property

TYPICAL PROPERTIES (1)      
MECHANICAL Value Unit Standard
Tensile Stress, yld, Type I, 50 mm/min 50 MPa ASTM D 638
Tensile Stress, brk, Type I, 50 mm/min 36 MPa ASTM D 638
Tensile Strain, yld, Type I, 50 mm/min 3 % ASTM D 638
Tensile Strain, brk, Type I, 50 mm/min 21 % ASTM D 638
Tensile Modulus, 50 mm/min 2470 MPa ASTM D 638
Flexural Stress, yld, 1.3 mm/min, 50 mm span 70 MPa ASTM D 790
Flexural Modulus, 1.3 mm/min, 50 mm span 2060 MPa ASTM D 790
Tensile Stress, yield, 50 mm/min 50 MPa ISO 527
Tensile Stress, break, 50 mm/min 38 MPa ISO 527
Tensile Strain, yield, 50 mm/min 3 % ISO 527
Tensile Strain, break, 50 mm/min 25 % ISO 527
Tensile Modulus, 1 mm/min 2300 MPa ISO 527
Flexural Stress, yield, 2 mm/min 70 MPa ISO 178
Flexural Modulus, 2 mm/min 2410 MPa ISO 178
Pencil Hardness test, 1kgf F - ASTM D 3363
IMPACT Value Unit Standard
Izod Impact, notched, 23°C 45 J/m ASTM D 256
Izod Impact, notched, -30°C 27 J/m ASTM D 256
Izod Impact, notched 80*10*4 +23°C 5 kJ/m² ISO 180/1A
Izod Impact, notched 80*10*4 -30°C 3 kJ/m² ISO 180/1A
THERMAL Value Unit Standard
Vicat Softening Temp, Rate B/50 78 °C ASTM D 1525
HDT, 1.82 MPa, 6.4 mm, unannealed 73 °C ASTM D 648
Vicat Softening Temp, Rate B/50 79 °C ISO 306
HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm 73 °C ISO 75/Af
PHYSICAL Value Unit Standard
Specific Gravity 1.15 - ASTM D 792
Melt Flow Rate, 220°C/10.0 kgf 38 g/10 min ASTM D 1238
Density 1.15 g/cm³ ISO 1183
Source GMD, last updated:03/20/2008    

Processing

Parameter    
Profile Extrusion Value Unit
Drying Temperature 75 - 85 °C
Drying Time 4 hrs
Maximum Moisture Content 0.02 %
Melt Temperature 200 - 230 °C
Barrel - Zone 1 Temperature 205 - 220 °C
Barrel - Zone 2 Temperature 210 - 225 °C
Barrel - Zone 3 Temperature 215 - 225 °C
Barrel - Zone 4 Temperature 215 - 225 °C
Hopper Temperature 60 - 80 °C
Adapter Temperature 200 - 225 °C
Die Temperature 210 - 225 °C
Calibrator Temperature 50 - 70 °C
Source GMD, last updated:03/20/2008  

 
 


Other related products we recommend:

For more information please download the datasheet

S-Plastic Geloy EXGY0049 ASA/PMMA 0  S-Plastics Geloy EXGY004.pdf

 

Get The Latest Quotation

 

First-level distribution source in South China

Reduce procurement costs, improve supply stability,

Help you find the most suitable engineering plastic materials

 

S-Plastic Geloy EXGY0049 ASA/PMMA 1Click to consult and get the latest quotation within 24 hours!

 

S-Plastic Geloy EXGY0049 ASA/PMMA 2

Recommended Products
Get in touch with us
Tel : 86-13925273675
Characters Remaining(20/3000)