S-Plastics Thermocomp PFB42U resin is a compound based on Nylon 6 resin containing Glassfiber and Glass Beads Additional features include
| TYPICAL PROPERTIES (1) | |||
| MECHANICAL | Value | Unit | Standard |
| Tensile Stress, break, 5 mm/min | 95 | MPa | ISO 527 |
| Tensile Strain, break, 5 mm/min | 4 | % | ISO 527 |
| Flexural Stress, break, 2 mm/min | 140 | MPa | ISO 178 |
| Flexural Modulus, 2 mm/min | 4400 | MPa | ISO 178 |
| IMPACT | Value | Unit | Standard |
| Izod Impact, unnotched 80*10*4 +23°C | 35 | kJ/m² | ISO 180/1U |
| Izod Impact, notched 80*10*4 +23°C | 5 | kJ/m² | ISO 180/1A |
| THERMAL | Value | Unit | Standard |
| HDT/Ae, 1.8 MPa Annealed 120°C, 2hrs | 170 | °C | ISO 75/Ae |
| PHYSICAL | Value | Unit | Standard |
| Mold Shrinkage, flow | 0.5 | % | S-Plastics Method |
| Density | 1.3 | g/cm³ | ISO 1183 |
| FLAME CHARACTERISTICS | Value | Unit | Standard |
| UL Compliant, 94HB Flame Class Rating (3)(4) | 1.6 | mm | UL 94 by GE |
| Source GMD, last updated:11/16/2007 | |||
| Parameter | ||
| Injection Molding | Value | Unit |
| Drying Temperature | 80 | °C |
| Drying Time | 4 | hrs |
| Maximum Moisture Content | 0.15 - 0.25 | % |
| Melt Temperature | 265 - 275 | °C |
| Front - Zone 3 Temperature | 275 - 290 | °C |
| Middle - Zone 2 Temperature | 265 - 275 | °C |
| Rear - Zone 1 Temperature | 250 - 260 | °C |
| Mold Temperature | 80 - 95 | °C |
| Back Pressure | 0.3 - 0.7 | MPa |
| Screw Speed | 30 - 60 | rpm |
| Source GMD, last updated:11/16/2007 | ||
Other related products we recommend:
|
For more information please download the datasheet |
|