| Melt Flow Rate, 260°C/2.16 Kgf | 29 |
|---|---|
| Melt Volume Rate, MVR At 260°C/2.16 Kg | 30cm³/10 Min |
| UV PerfoImprovedrmance | Improved |
| Aesthetically And Physically | Improved |
| Packaging Details | 25KG/bag |
| Density | 1.08 |
|---|---|
| Mold Shrinkage, Flow | 0.82 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 9 |
|---|---|
| Oxygen Index (LOI) | 47 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 9 |
|---|---|
| Oxygen Index (LOI) | 50 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 17.8 |
|---|---|
| Oxygen Index (LOI) | 47 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 7.6 |
|---|---|
| Glass Fiber | 30% |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 11 |
|---|---|
| Electroplatability | Enhanced |
| Mold Release | Internal |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Melt Flow Rate, 337°C/6.6 Kgf | 9.5 |
|---|---|
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Supply Ability | To be negotiated |
| Melt Volume Rate, MVR At 300°C/10.0 Kg | 50 |
|---|---|
| UL Recognized, 94V-1 Flame Class Rating (3) | 2.5 |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Melt Flow Rate, 337°C/6.6 Kgf | 24 |
|---|---|
| ECO Conforming | Yes |
| Packaging Details | 25KG/bag |
| Delivery Time | To be negotiated |
| Payment Terms | L/C, T/T, Western Union, MoneyGram |