S-Plastics Thermocomp Noryl_EXCP0104 resin is a 10% carbon fibre filled PPO/PS injection moulding resin.
| MECHANICAL | Value | Unit | Standard |
| Tensile Stress, break, 5 mm/min | 70 | MPa | ISO 527 |
| Tensile Strain, break, 5 mm/min | 1.3 | % | ISO 527 |
| Tensile Modulus, 1 mm/min | 6800 | MPa | ISO 527 |
| Flexural Modulus, 2 mm/min | 6300 | MPa | ISO 178 |
| IMPACT | Value | Unit | Standard |
| Izod Impact, unnotched 80*10*4 +23°C | 12 | kJ/m² | ISO 180/1U |
| Izod Impact, notched 80*10*4 +23°C | 5 | kJ/m² | ISO 180/1A |
| ELECTRICAL | Value | Unit | Standard |
| Volume Resistivity | 2.E+06 | Ohm-cm | IEC 60093 |
| Surface Resistivity, ROA | 6.E+04 | Ohm | IEC 60093 |
| Source GMD, last updated:09/20/2001 | |||
| Parameter | ||
| Injection Molding | Value | Unit |
| Drying Temperature | 100 - 120 | °C |
| Drying Time | 2 - 3 | hrs |
| Melt Temperature | 280 - 300 | °C |
| Nozzle Temperature | 260 - 280 | °C |
| Front - Zone 3 Temperature | 280 - 300 | °C |
| Middle - Zone 2 Temperature | 260 - 280 | °C |
| Rear - Zone 1 Temperature | 240 - 260 | °C |
| Hopper Temperature | 60 - 80 | °C |
| Mold Temperature | 80 - 120 | °C |
| Source GMD, last updated:09/20/2001 | ||
Other related products we recommend:
|
For more information please download the datasheet |
|
| S-Plastics Thermocomp Noryl_EXCP0104.pdf | |
|
Get The Latest Quotation
First-level distribution source in South China Reduce procurement costs, improve supply stability, Help you find the most suitable engineering plastic materials
|
![]()