S-Plastics Thermocomp OFM66 resin is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Mineral. Added features of this
material include: Low Warpage.
| TYPICAL PROPERTIES (1) | |||
| MECHANICAL | Value | Unit | Standard |
| Tensile Stress, break | 115 | MPa | ASTM D 638 |
| Tensile Strain, break | 2.8 | % | ASTM D 638 |
| Flexural Stress | 172 | MPa | ASTM D 790 |
| Flexural Modulus | 17940 | MPa | ASTM D 790 |
| IMPACT | Value | Unit | Standard |
| Izod Impact, unnotched, 23°C | 170 | J/m | ASTM D 4812 |
| Izod Impact, notched, 23°C | 37 | J/m | ASTM D 256 |
| THERMAL | Value | Unit | Standard |
| HDT, 0.45 MPa, 3.2 mm, unannealed | 276 | °C | ASTM D 648 |
| HDT, 1.82 MPa, 3.2mm, unannealed | 254 | °C | ASTM D 648 |
| PHYSICAL | Value | Unit | Standard |
| Density | 1.92 | g/cm³ | ASTM D 792 |
| ELECTRICAL | Value | Unit | Standard |
| Dissipation Factor, 1 MHz | @ 1MHz0.002 | - | ASTM D 150 |
| Source GMD, last updated:09/24/2008 | |||
| Parameter | ||
| Injection Molding | Value | Unit |
| Drying Temperature | 120 - 150 | °C |
| Drying Time | 4 | hrs |
| Melt Temperature | 315 - 320 | °C |
| Front - Zone 3 Temperature | 330 - 345 | °C |
| Middle - Zone 2 Temperature | 320 - 330 | °C |
| Rear - Zone 1 Temperature | 305 - 315 | °C |
| Mold Temperature | 140 - 165 | °C |
| Back Pressure | 0.2 - 0.3 | MPa |
| Screw Speed | 30 - 60 | rpm |
| Source GMD, last updated:09/24/2008 | ||