S-Plastics Lexan RL7609resin is PRELIMINARY DATA. UV-stabilized, ECO-FR, PC. Extrusion applications.
| MECHANICAL | Value | Unit | Standard |
| Tensile Stress, yld, Type I, 50 mm/min | 62 | MPa | ASTM D 638 |
| Tensile Stress, brk, Type I, 50 mm/min | 64 | MPa | ASTM D 638 |
| Tensile Strain, yld, Type I, 50 mm/min | 6.2 | % | ASTM D 638 |
| Tensile Strain, brk, Type I, 50 mm/min | 101 | % | ASTM D 638 |
| Tensile Modulus, 50 mm/min | 2500 | MPa | ASTM D 638 |
| Flexural Stress, yld, 1.3 mm/min, 50 mm span | 100 | MPa | ASTM D 790 |
| Flexural Modulus, 1.3 mm/min, 50 mm span | 2320 | MPa | ASTM D 790 |
| IMPACT | Value | Unit | Standard |
| Izod Impact, notched, 23°C | 849 | J/m | ASTM D 256 |
| Instrumented Impact Total Energy, 23°C | 73 | J | ASTM D 3763 |
| THERMAL | Value | Unit | Standard |
| HDT, 0.45 MPa, 3.2 mm, unannealed | 141 | °C | ASTM D 648 |
| HDT, 1.82 MPa, 3.2mm, unannealed | 128 | °C | ASTM D 648 |
| Relative Temp Index, Elec | 80 | °C | UL 746B |
| Relative Temp Index, Mech w/impact | 80 | °C | UL 746B |
| Relative Temp Index, Mech w/o impact | 80 | °C | UL 746B |
| PHYSICAL | Value | Unit | Standard |
| Specific Gravity | 1.19 | - | ASTM D 792 |
| FLAME CHARACTERISTICS | Value | Unit | Standard |
| UL Recognized, 94V-0 Flame Class Rating (3) | 1.9 | mm | UL 94 |
| Source GMD, last updated:09/28/2000 | |||
|