S-Plastics Lexan I2220 resin is General purpose polycarbonate with melt flow rate of 10.5
TYPICAL PROPERTIES (1) | |||
MECHANICAL | Value | Unit | Standard |
Tensile Stress, yld, Type I, 50 mm/min | 62 | MPa | ASTM D 638 |
Tensile Stress, brk, Type I, 50 mm/min | 68 | MPa | ASTM D 638 |
Tensile Strain, yld, Type I, 50 mm/min | 7 | % | ASTM D 638 |
Tensile Strain, brk, Type I, 50 mm/min | 130 | % | ASTM D 638 |
Flexural Stress, yld, 1.3 mm/min, 50 mm span | 96 | MPa | ASTM D 790 |
Flexural Modulus, 1.3 mm/min, 50 mm span | 2340 | MPa | ASTM D 790 |
Tensile Stress, yield, 50 mm/min | 63 | MPa | ISO 527 |
Tensile Stress, break, 50 mm/min | 70 | MPa | ISO 527 |
Tensile Strain, yield, 50 mm/min | 6 | % | ISO 527 |
Tensile Strain, break, 50 mm/min | 110 | % | ISO 527 |
Tensile Modulus, 1 mm/min | 2350 | MPa | ISO 527 |
Flexural Stress, yield, 2 mm/min | 90 | MPa | ISO 178 |
Flexural Modulus, 2 mm/min | 2300 | MPa | ISO 178 |
IMPACT | Value | Unit | Standard |
Izod Impact, unnotched, 23°C | 3204 | J/m | ASTM D 4812 |
Izod Impact, notched, 23°C | 801 | J/m | ASTM D 256 |
Instrumented Impact Energy @ peak, 23°C | 63 | J | ASTM D 3763 |
Izod Impact, notched 80*10*4 +23°C | 12 | kJ/m² | ISO 180/1A |
Izod Impact, notched 80*10*4 -30°C | 10 | kJ/m² | ISO 180/1A |
Charpy -30°C, Unnotch Edgew 80*10*4 sp=62mm | NB | kJ/m² | ISO 179/1eU |
THERMAL | Value | Unit | Standard |
Vicat Softening Temp, Rate B/50 | 154 | °C | ASTM D 1525 |
HDT, 0.45 MPa, 6.4 mm, unannealed | 137 | °C | ASTM D 648 |
HDT, 1.82 MPa, 6.4 mm, unannealed | 132 | °C | ASTM D 648 |
CTE, 23°C to 80°C, flow | 7.E-05 | 1/°C | ISO 11359-2 |
CTE, 23°C to 80°C, xflow | 6.8E-05 | 1/°C | ISO 11359-2 |
Vicat Softening Temp, Rate B/50 | 141 | °C | ISO 306 |
Vicat Softening Temp, Rate B/120 | 142 | °C | ISO 306 |
HDT/Ae, 1.8 MPa Edgew 120*10*4 sp=100mm | 125 | °C | ISO 75/Ae |
PHYSICAL | Value | Unit | Standard |
Specific Gravity | 1.2 | - | ASTM D 792 |
Water Absorption, 24 hours | 0.15 | % | ASTM D 570 |
Water Absorption, equilibrium, 23C | 0.35 | % | ASTM D 570 |
Mold Shrinkage, flow, 3.2 mm | 0.5 - 0.7 | % | S-Plastics Method |
Melt Flow Rate, 300°C/1.2 kgf | 10.5 | g/10 min | ASTM D 1238 |
Density | 1.2 | g/cm³ | ISO 1183 |
Water Absorption, (23°C/sat) | 0.35 | % | ISO 62 |
Moisture Absorption (23°C / 50% RH) | 0.15 | % | ISO 62 |
Melt Volume Rate, MVR at 300°C/1.2 kg | 12 | cm³/10 min | ISO 1133 |
Source GMD, last updated:02/16/2007 |
Parameter | ||
Injection Molding | Value | Unit |
Drying Temperature | 120 | °C |
Drying Time | 3 - 4 | hrs |
Drying Time (Cumulative) | 48 | hrs |
Maximum Moisture Content | 0.02 | % |
Melt Temperature | 295 - 315 | °C |
Nozzle Temperature | 290 - 310 | °C |
Front - Zone 3 Temperature | 295 - 315 | °C |
Middle - Zone 2 Temperature | 280 - 305 | °C |
Rear - Zone 1 Temperature | 270 - 295 | °C |
Mold Temperature | 70 - 95 | °C |
Back Pressure | 0.3 - 0.7 | MPa |
Screw Speed | 40 - 70 | rpm |
Shot to Cylinder Size | 40 - 60 | % |
Vent Depth | 0.025 - 0.076 | mm |
Source GMD, last updated:02/16/2007 |
For more information please download the datasheet |
|
![]() |
S-Plastics Lexan I2220.pdf |